Mg-Ca0.3 Electrochemical Activity Exposed to Hank’s Physiological Solution and Properties of Ag-Nano-Particles Deposits

This work compares the degradation of Mg and Mg-Ca0.3 alloy when they are exposed for 14 days to Hank’s solution at 37 °C. A combination of immersion test, electrochemical techniques (PDP, EIS, EN), and surface characterization methods (SEM-EDS, XRD, and XPS) were carried out. The pH change over tim...