Preparación de películas delgadas de As2S3 por depósito químico con perspectivas de aplicación en celdas solares

In this paper we obtained thin films of As2S3 by chemical bath deposition. The films were prepared at a temperature of 80ºC for 3 hours each deposit. They were thermally treated at 180ºC and 250ºC for 30 minutes for 1 hour, respectively. The energy gap was calculated 2.9 eV. The conductivity was aro...

Descripción completa

Detalles Bibliográficos
Autores principales: Benítez Garza, Ángel Salvador, Lugo, S., Peña Méndez, Yolanda, Elizondo, Perla, Garza, T.
Formato: Artículo
Lenguaje:Spanish / Castilian
Publicado: Universidad Autónoma de Nuevo León 2010
Materias:
Acceso en línea:http://eprints.uanl.mx/13333/1/Art5.pdf